It was found that undesirable Ï phase which forms between Fe and V is not created during the laser welding process because of high cooling rates. However, the zones whose composition corresponds to Ï homogeneity range are crack-susceptible, so the best choice is to reduce the V content in steel/vanadium melted zone below Ï phase formation limit. In the same time, the proportion between V and Ti in Ti6Al4V/vanadium melted zones does not influence mechanical properties as these elements form ideal solid solution.