The microstructures and mechanical properties of Mg–5.3Zn–0.2Ca–0.5Ce (wt%) alloy fabricated by semi-continuous casting were investigated. The as-cast alloy consists of α-Mg, Ca2Mg6Zn3 and T′1 phase with orthorhombic structure (a=0.57 nm, b=0.75 nm and c=1.00 nm). T′1 phase mainly distributes at the triple conjunctions while the Ca2Mg6Zn3 at the grain boundaries. The as-cast alloy exhibits high strength retention due to the stable Ca2Mg6Zn3 and T′1 phase at the grain boundaries.