Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1576500 | Materials Science and Engineering: A | 2013 | 8 Pages |
Abstract
Cyclic deformation and fatigue of extruded rare-earth Mg-8.0Gd-3.0Y-0.5%Zr (GW83) magnesium (Mg) alloy were experimentally investigated by carrying out fully reversed strain-controlled tension-compression experiments along the extrusion direction with the strain amplitudes varying from 0.275% to 5.0%. Monotonic tension and compression stress-strain curves display a smooth transition from elastic to elastic-plastic deformation and exhibit a fairly yielding symmetry. Different from conventional Mg alloys, the material shows near-symmetric stress-strain hysteresis loops and marginal cyclic hardening with almost zero mean stress in the fully reversed strain-controlled experiments conducted. With increasing number of loading cycles, a transition of stress-strain response from concave-down shape to sigmoidal shape occurs in both tension and compression reversals when the strain amplitudes are larger than 2.0%. The strain-life fatigue curve displays a similar feature to that of conventional Mg alloys: A detectable transition from low-cycle region to high-cycle region occurs at a kink point in the vicinity of a strain amplitude of 0.75%. The cyclic deformation and fatigue properties of GW83 Mg alloy and the associated cyclic deformation mechanism are discussed and compared with those of a typical conventional Mg alloy.
Related Topics
Physical Sciences and Engineering
Materials Science
Materials Science (General)
Authors
Fenghua Wang, Jie Dong, Yanyao Jiang, Wenjiang Ding,