The fracture of Ti/Ti joints was found to mainly propagate along the grain boundary. In the MAO-TiO2/MAO-TiO2 and MAO-TiO2/Ti samples, the failure mode transitioned from MAO-TiO2 layer/Ti interfacial fracture to fracture within the active solder.