Article ID Journal Published Year Pages File Type
1577065 Materials Science and Engineering: A 2012 8 Pages PDF
Abstract

Boron concentration profile around prior austenite grain boundaries in Fe-0.05C–0.5Mo–0.001B (mass%) is examined by using aberration corrected STEM–EELS. Tilt series measurements of line analysis with a thin specimen (<30 nm) and the principal component analysis (PCA) are performed to obtain the precise distribution of boron around the boundary. The concentration on the grain boundary reaches beyond 8 at% and the distribution width is about 1.2 nm. The effects of the boundary inclination and the specimen thickness are also examined by calculation based on the Gaussian broadening model. The obtained concentration profile implies that the boron segregation in the present material is formed by ‘non-equilibrium segregation mechanism’.

Related Topics
Physical Sciences and Engineering Materials Science Materials Science (General)
Authors
, , ,