Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1581538 | Materials Science and Engineering: A | 2008 | 6 Pages |
Abstract
Refinement and modification performance of Al-Ti-B master alloy alone or with Al-P master alloy on primary Mg2Si in Al-12.67% Mg-10.33% Si alloy was investigated in this paper. The experimental results show that perfect effect can be obtained after addition of 1% Al-5Ti-1B master alloy into the Al-Mg-Si alloy. The morphologies of primary Mg2Si particulates change from dendritic to polygonal shape, and their average sizes decrease from â¼100 to â¼20 μm. The ultimate tensile strength of the alloy increases. EPMA and TEM results show that TiB2 particles act as the nuclei of primary Mg2Si. Crystal lattice correspondence indicates TiB2 has a good lattice matching coherence relationship with Mg2Si, and the disregistry is only 4.64%. Furthermore, the addition of Al-5Ti-1B master alloy can significantly improve the refinement and modification effect of AlP on primary Mg2Si. It is also found that coupling particles of AlP and TiB2 exist in the center of primary Mg2Si.
Related Topics
Physical Sciences and Engineering
Materials Science
Materials Science (General)
Authors
Chong Li, Xiangfa Liu, Guohua Zhang,