| Article ID | Journal | Published Year | Pages | File Type |
|---|---|---|---|---|
| 1581686 | Materials Science and Engineering: A | 2009 | 5 Pages |
Abstract
Fatigue strength and life of weldment at high temperatures are important for the materials in power plants. The fatigue crack growth rate is accelerated by oxidation. Similarly, the high-temperature fatigue life is influenced by oxidation. The base metal, the weld metal and the heat-affected zone (HAZ) of the P122 (Cr-Mo steel) weldment were oxidized between 600 °C and 700 °C for up to 500 h in air, and their oxidation behavior was examined. The oxidation resistance increased in the order of HAZ, base metal and weld metal. The scales were mainly Fe2O3. Fatigue tests were performed to measure the fatigue crack growth rate in the range of low stress intensity factor, and the results are discussed from the viewpoint of different microstructures and oxidation.
Keywords
Related Topics
Physical Sciences and Engineering
Materials Science
Materials Science (General)
Authors
S.Y. Bae, H.G. Kang, H.S. Yun, C.W. Kim, D.B. Lee, B.S. Lim,