Furthermore, an increase in the volume fraction of Ta (0-6Â vol%) in the BMGCs does not encourage the formation of the harmful crystalline phase in the amorphous matrix after the laser welding process. It is observed that, other than the IL (ZrCu) on the micro-sized Ta particles, no other type of crystalline is observed in the amorphous matrix of the laser-welded BMGCs.