Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1605405 | Journal of Alloys and Compounds | 2016 | 4 Pages |
Abstract
SEM images of corroded specimens. (a) PN: Vair = 0L/min; (b) PON: Vair = 0.3L/min. (a) clearly shows that there exist many corrosion pits distributed on the surface due to the pores existed in the compound layer. While there exists no corrosion pits in the image of PON treated sample. (b) due to the protection from chemically stable and compact Fe3O4 formed in the compound layer, corresponding to the optimum corrosion resistance.630
Related Topics
Physical Sciences and Engineering
Materials Science
Metals and Alloys
Authors
Jiqiang Wu, Han Liu, Jingcai Li, Xingmei Yang, Jing Hu,