Abstract
The electrooptic and piezoelectric coupling effects in tetragonal relaxor-based ferroelectric 0.62Pb(Mg1/3Nb2/3)O3-0.38PbTiO3 (PMN-0.38PT) and 0.88Pb(Zn1/3Nb2/3)O3-0.12PbTiO3 (PZN-0.12PT) single-domain crystals have been analyzed by the coordinate transformation. The orientation dependence of the electrooptic and half-wave voltage was calculated based on the full sets of refractive indices, electrooptic and piezoelectric coefficients. The optimum orientation cuts for achieving the best electrooptic coefficient and half-wave voltage were found. The lowset half-wave voltage is only 76Â V for the PMN-0.38PT single-domain crystal. Compared to commonly used electrooptic crystal LiNbO3, tetragonal relaxor-PT ferroelectric single-domain crystals are much superior for optical modulation applications because of their much higher linear electrooptic coefficients and substantially lower half-wave voltages when the piezoelectric strain influence is considered.
Related Topics
Physical Sciences and Engineering
Materials Science
Metals and Alloys
Authors
Enwei Sun, Shijing Sang, Zhongyuan Yuan, Xudong Qi, Rui Zhang, Wenwu Cao,