| Article ID | Journal | Published Year | Pages | File Type |
|---|---|---|---|---|
| 1614746 | Journal of Alloys and Compounds | 2013 | 6 Pages |
Abstract
⺠Mg-1% Mn (M1) and M1-1.6% Sr (M1-1.6Sr) alloys were extruded at 300, 350 and 400 °C. ⺠Extrusion at 300 °C develops weaker texture in alloy M1 whereas extrusion at 350 and 400 °C gives basal fiber texture in M1. ⺠Sr addition to alloy M1 results in randomization of texture due to particle stimulated nucleation (PSN) at all extrusion temperatures.
Related Topics
Physical Sciences and Engineering
Materials Science
Metals and Alloys
Authors
Hemant Borkar, Raynald Gauvin, Mihriban Pekguleryuz,