Abstract
⺠Lattice strain decreases and crystallite size increases with annealing temperature. ⺠Coercivity follows the Herzer's random anisotropy model in the temperature range 450-600 °C. ⺠Maximum saturation magnetization of 77.04 emu/g is obtained after heat treatment at 750 °C.