⺠Barium silicates and hexacelsian ceramics are prepared at the sintering temperature of 850-940 oC. ⺠The BaO-B2O3 compositions can availably decrease the sintering temperature the barium silicate and hexacelsian ceramics. ⺠The presence of barium silicates and SiO2 crystal in the ceramics can urge a higher CTE (11-17 ppm oCâ1). ⺠The formation of a hexacelsian phase can achieve a low permittivity and loss (permittivity: 7.1-7.4; loss: 5-7 Ã 10â4).