Abstract
⺠(Fe50âx/2Co50âx/2)Snx mixtures are mechanically alloyed for x â¤Â 33 at.%. ⺠As-ground powders are studied by X-ray diffraction and 57Fe and 119Sn Mössbauer spectroscopy. ⺠Supersaturated solutions of Sn in disordered bcc FeCo alloys are formed in our dynamical conditions up to x â¤Â 20 at.%. ⺠This maximum Sn solubility found is much larger than the equilibrium solubility which is about 0.5 at.%. ⺠The mean 119Sn hyperfine field in the bcc alloys is essentially constant with x and equal to 9.6 T at room temperature.
Keywords
Related Topics
Physical Sciences and Engineering
Materials Science
Metals and Alloys
Authors
J.M. Loureiro, B.F.O. Costa, G. Le Caër,