Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1617027 | Journal of Alloys and Compounds | 2011 | 6 Pages |
Abstract
⺠The structural transition from tetragonal to cubic lattice structure occurs around x = 1.2 wt.% in Sr2FexMo2-xO6 (0.8 â¤Â x â¤Â 1.5). ⺠The maximum degree of Fe/Mo ordering(ηmax), Saturation magnetization (Ms) and percentage of magnetoresistance (MR%) is maximum at x = 1.0 wt.% and decreases as x deviates from 1.0 in Sr2FexMo2-xO6 (0.8 â¤Â x â¤Â 1.5). ⺠Concentration of anti site defects (ASDs) is minimum at x = 1.0 wt.% and increases as x deviates from 1.0 in Sr2FexMo2-xO6 (0.8 â¤Â x â¤Â 1.5). ⺠Different resistivity behavior have been observed at x â¤Â 1.2 wt.% and x > 1.2 wt.% samples of Sr2FexMo2-xO6 (0.8 â¤Â x â¤Â 1.5).
Keywords
Related Topics
Physical Sciences and Engineering
Materials Science
Metals and Alloys
Authors
Y. Markandeya, K. Suresh, G. Bhikshamaiah,