Article ID Journal Published Year Pages File Type
1620988 Journal of Alloys and Compounds 2010 7 Pages PDF
Abstract

The formation of intermetallic compounds and the shear strength of Sn–Zn–Bi solder alloys with various (0, 1, 3, 5 and 7 wt%) weight percentages of Sn–Ag–Cu were investigated on Au/Ni metallized Cu pads depending on the number of reflow cycles. In Sn–Zn–Bi solder joints, scallop-shaped AuZn3 intermetallic compound (IMC) particles were found at the interfaces and in the solder ball regions, fine Bi- and needle-shaped Zn-rich phase were observed in the Sn matrix. After Sn–Ag–Cu additions, an additional Ag–Zn intermetallic compound layer was adhered to the top surface of the AuZn3 layer at the interface and fine spherical-shaped AgZn3 intermetallic compound particles were detected in the solder ball regions together with Bi- and Zn-rich phase volumes. After the addition of Sn–Ag–Cu, the shear strength of Sn–Zn–Bi solder joints increased due to the formation of the fine AgZn3 intermetallic compound particles. The shear strengths of Sn–Zn–Bi and Sn–Zn–Bi/7 wt% Sn–Ag–Cu solder joints after one reflow cycle were about 44.5 and 53.1 MPa, respectively and their shear strengths after eight reflow cycles were about 43.4 and 51.6 MPa, respectively.

Related Topics
Physical Sciences and Engineering Materials Science Metals and Alloys
Authors
, , , , ,