Article ID Journal Published Year Pages File Type
1621899 Journal of Alloys and Compounds 2009 4 Pages PDF
Abstract

The Seebeck coefficients, electrical resistivities, and total thermal conductivities are reported for temperatures between 10 and 300 K for p-type Bi–Sb alloys made by Sn-doping at the 5% level or below. Alloys are investigated for Sb contents at both extremes of the semiconducting region of the Bi–Sb alloy solid solution, 7–10% Sb and 18–20% Sb. The behavior of all the alloys is relatively similar, and the best p-type material found, Bi0.885Sb0.075Sn0.04, has a maximum thermoelectric figure of merit of ZT = 0.08 at 200 K. The thermoelectric efficiency of the optimal n–p couple in this alloy system peaks at ZT = 0.13 at a temperature of 200 K.

Related Topics
Physical Sciences and Engineering Materials Science Metals and Alloys
Authors
, ,