Article ID Journal Published Year Pages File Type
1623490 Journal of Alloys and Compounds 2009 6 Pages PDF
Abstract

Starting mixtures of ZnO, TiO2 and MgO (0, 1.25 and 2.5 wt.% MgO) powders were mechanically activated for 15 min in a planetary ball mill. The powders obtained were sintered non-isothermally to temperatures between 800 and 1100 °C and then held at those temperatures for 120 min. Analysis of the influence of MgO addition on the synthesis of zinc–titanate ceramics showed that its addition increased slightly the temperature at which the reaction process started, accelerated the reaction and resulted in higher sample densities. These results were correlated with the results of structural characterization using X-ray powder diffraction method and SEM analysis. Also, the results of electric resistivity, capacitance and loss tangent of the sintered samples were obtained.

Related Topics
Physical Sciences and Engineering Materials Science Metals and Alloys
Authors
, , , , , ,