Abstract
To resolve the difficulty in slag formation during steelmaking with low silicon hot metal and to increase productivity, a new 5-hole lance was developed by increasing oxygen flow from 50 000 m3/h to 60 000 m3/h. Synthetic slag was added to adjust the slag composition. The problems such as difficulty in dephosphorization and slag adhesion to oxygen lance and hood were settled. Steel production and metal yield were increased and the nozzle life was prolonged through these techniques.
Related Topics
Physical Sciences and Engineering
Materials Science
Metals and Alloys
Authors
JIANG Xiao-fang, WANG Ming-lin, YANG Wen-yuan, GAN Yong, WANG Ying-jun, YU Zu-da,