Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1639376 | Transactions of Nonferrous Metals Society of China | 2009 | 5 Pages |
Abstract
Microstructures of as-cast Al-Mg-Si-Mn alloys with and without Sc and Zr were investigated by optical microscopy, scanning electronic microscopy(SEM) and energy dispersion spectrum analysis. Addition of 0.2%–0.4% Sc can refine the grain size and change the growth morphology from dendritic to fine equi-axial crystal. The higher the addition of Sc, the finer the as-cast grain size. The tensile strength is increased by more than 30% with 0.4% Sc. Moreover, an addition of 0.1%–0.2% Zr is able to refine grain size and change the growth morphology from dendritic to equi-axial grain too, but less effective. However, Zr is found to increase the ductility of the cast alloys, and the elongation is increased to 11.97% with 0.2% Zr.
Related Topics
Physical Sciences and Engineering
Materials Science
Metals and Alloys