Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1641217 | Materials Letters | 2016 | 5 Pages |
•Aqueous solution chemical method to prepare single layer Cu1.5Mn1.5O4 spinel films.•Only one dipping/annealing cycle is employed to fabricate spinel films.•Cu1.5Mn1.5O4 spinel phase can be obtained at the annealing temperature of 500 °C.•Single layer films exhibit αs=0.906–0.915 and ε100=0.146–0.172.
Spinel Cu1.5Mn1.5O4 thin films were fabricated by one step sol-gel dip-coating method using aqueous solution. The effect of deposition parameters on thickness, surface feature, and optical property of thin films was systematically studied. The results revealed that the increased withdrawal speeds and high concentration of metal ions in precursor were conducive to obtaining thicker films which exhibited excellent solar absorptance. Furthermore, the surface feature derived from the different concentrations of metal ions had a significant effect on optical behavior of the thin film. Consequently, excellent spectral selectivity of the thin film would be achieved by tuning those deposition parameters.