| Article ID | Journal | Published Year | Pages | File Type |
|---|---|---|---|---|
| 1648006 | Materials Letters | 2011 | 4 Pages |
Abstract
The Sr1.99MgSi2O7: Eu2+0.01, and Sr1.97MgSi2O7: Eu2+0.01, R3+0.02 (R: Dy, Er) are synthesized via high temperature solid-state reaction. The sample without codoping shows the highest luminescent efficiency, leading to the strongest emission intensity. Both Dy3+ and Er3+ enhance the afterglow properties. Compared with Dy3+, sample doped with Er3+ shows a longer afterglow duration because of a deeper trap and it may be the optimum codopant for Sr2MgSi2O7: Eu2+ long afterglow phosphors.
Related Topics
Physical Sciences and Engineering
Materials Science
Nanotechnology
Authors
Haoyi Wu, Yihua Hu, Li Chen, Xiaojuan Wang,