Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1653218 | Materials Letters | 2007 | 4 Pages |
Abstract
The microstructure performance of Mg/Al TIG welded joint was studied by means of metallography, micro-hardness test and SEM. The test results indicate that the structure close to weld metal is columnar crystals, which grow into the weld metal. The weld metal was mainly composed of dendrite crystal. The micro-hardness near the fusion zone of Mg side is about HM 275–300. The brittleness phase with high hardness may be formed near the fusion zone. The fracture surface of Mg side shows a river pattern, which is a typical cleavage morphology. There are some hydrogen (H2) air holes in the fracture of Mg side.
Related Topics
Physical Sciences and Engineering
Materials Science
Nanotechnology
Authors
Peng Liu, Yajiang Li, Haoran Geng, Juan Wang,