SrAl2O4: Eu2+, Dy3+ nanometer phosphors were synthesized by detonation method. The particle morphology and optical properties of detonation soot that was heated at different temperatures (600–1100 °C) had been studied systematically by X-ray diffraction (XRD) and transmission electron microscopy (TEM). Results indicated SrAl2O4: Eu2+, Dy3+ nanometer powders in monoclinic system (a = 8.442, b = 8.822, c = 5.160, β = 93.415) can be synthesized by detonation method, when detonation soot was heated at 600–800 °C. The particle size of SrAl2O4: Eu2+, Dy3+ is 35 ± 15 nm. Compared with the solid-state reaction and sol-gel method, synthesis temperature of the detonation method is lower about 500 and 200 °C respectively. After being excited under UN lights, detonation soot and that heated at 600–1100 °C can emit a green light.