⺠ZnS films were deposited by chemical bath deposition method at different temperatures. ⺠The ZnS film thicknesses are about 73-200 nm. ⺠Annealing makes some particles grow up and the surface smooth. ⺠The annealed films contain Zn and S and have a microcrystalline structure. ⺠The ZnS films had high transmittance of about 78% in the range of 350-800 nm.