Abstract
Defects and cracks in thin film barriers that are coated on polymers allow the leakage of reactive species through the polymer substrate. Fluorescent tags have been developed to visualize defects and cracks in thin film barriers and to inspect rapidly the barrier quality with minimal sample preparation. For Al2O3 films with a thickness of 25 nm deposited on polyethylene naphthalate polymer substrates using atomic layer deposition techniques, the fluorescent tags have identified cracks ~ 20 nm in width after applied strain and have observed individual defects as small as ~ 200 nm in diameter.