Oxyfluoride glasses 16Na2O-9NaF-5LaF3-7Al2O3-63SiO2 (mol%) activated with 3% terbium, dysprosium, praseodymium and neodymium fluorides have been prepared and studied by differential thermal analysis, cathodoluminescence, X-ray induced luminescence, X-ray diffraction, scanning electron microscopy and energy dispersive X-ray spectroscopy. We found out that the presence of crystalline phase enhances the X-ray induced luminescence intensity. X-ray induced luminescence is the most intense for the sample activated with terbium and treated at 700 °C, whereas the praseodymium and neodymium activated samples have the fastest decay times.