Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1696501 | Applied Clay Science | 2007 | 10 Pages |
Abstract
Re-optimisation of collector dosage based on these improved pretreatment conditions helped to remove more titanoferrous impurities. Lowest product titania achieved is 0.35% from a feed value of 1.06%. The flotation product measured 85% ISO brightness at a clay recovery of 86.4%. The brightness was further improved to 85.7% by reductive bleaching.
Keywords
Related Topics
Physical Sciences and Engineering
Earth and Planetary Sciences
Geochemistry and Petrology
Authors
P. Raghavan, S. Chandrasekhar, V. Vogt, E. Gock, N. Suresh,