Erosive wear of hydro turbine runners depends upon different parameters such as size, hardness and concentration of silt particles, velocity of flow, properties of the base material of the turbine components and operating hours of the turbine. Various researchers have conducted experiments to study the effect of these parameters on erosive wear. Most of these experiments were on small-size samples at different types of test rigs to simulate the flow conditions in turbines, however actual flow conditions and the phenomenon of erosive wear are too complex to simulate. Under the present study, effect of these parameters on erosion in actual conditions has been investigated experimentally. An extensive experimental study has been carried out on a small scale Pelton turbine. Based on the experimental data collected for different parameters, correlations have been developed for wear rate of Pelton turbine buckets as a function of critical parameters, i.e., size and concentration of silt particles and jet velocity.

Related Topics
Physical Sciences and Engineering Energy Energy (General)
Authors
, ,