1796251 Journal of Crystal Growth 2006 4 Pages PDF
Abstract

This paper reported the growth of potassium titanyl phosphate (KTiOPO4 or KTP) crystals by hydrothermal method. The KTP crystals were grown in 2.0 mol/l K2HPO4+0.1 mol/l KH2PO4+1 wt% H2O2 solution using crushed flux KTP crystals as nutrients. The KTP crystals with dimension up to 14.5×28×17 mm3 and excellent quality were obtained. The growing rate of KTP crystals along (0 1 1) was 0.15 mm/day. The damage threshold value of the grown KTP crystal was up to 9.5 GW/cm2 for 1064 nm (TEM00, 10 ns). The transmittance was over 80% in the range of 450–2500 nm.