Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1812622 | Physica B: Condensed Matter | 2009 | 7 Pages |
Abstract
The frequency and temperature dependent conductivity measurements for heat treated titanium bismuth silicate glasses of composition 5TiO2·(95âx)Bi2O3·xSiO2 (x=30, 40 and 50 mol%) have been carried out by using impedance spectroscopy in the frequency range from 20 Hz to 1 MHz and temperature range from 210 to 360 °C. An enhancement in conductivity of about 101-102 order is obtained in heat treated sample as compared to parent glass. In heat treated glass samples conductivity increases as the concentration of bismuth oxide increases. The absence of maxima in the dielectric permittivity (εâ²) spectra indicates the non-ferroelectric behavior of the samples. The loss factor (tan δ) is associated with the losses by conduction and it decreases with decrease in bismuth oxide. The effect of temperature on scaling of dielectric modulus indicates that the conductivity relaxation mechanism is temperature independent. The relaxation observed for the Mâ³(Ï) or Zâ³(Ï) functions is correlated to both localized and long range conduction. The overlapping of the Mâ³(Ï) and Zâ³(Ï) peaks at a given temperature suggests the same activation energy and existence of a single carrier that are related to the same relaxation process.
Related Topics
Physical Sciences and Engineering
Physics and Astronomy
Condensed Matter Physics
Authors
S. Duhan, S. Sanghi, A. Agarwal, A. Sheoran, S. Rani,