Article ID Journal Published Year Pages File Type
227375 Journal of Industrial and Engineering Chemistry 2014 7 Pages PDF
Abstract

Using waste LCD glass as a base material helped developed the manufacturing process of the spherical foamed body and its varied functionality. Also, the manufactured spherical foamed body showed great performance as a water treatment media. By mixing 90 wt% of waste LCD glass, 100 parts by weight of glass mixture that has 10 wt% kaolinite as a shaping agent, 1.0 part by weight of carbon foaming agent, and mixture of each 1.5 parts by weight of Na2CO3, CaCO3 and Na2SO4 as foaming agents and the MgO as a parting agent for 10 min of foaming calcination in the rotary kiln at 970–1000 °C, the spherical foamed body can be manufactured effectively. The manufactured spherical foamed body performed as a great water treatment media by showing 70.5% of SS removal efficiency, 56.1% of BOD removal efficiency, 57.5% of COD removal efficiency, 28.6% of denitrification and 49.8% of phosphorous removal.

Related Topics
Physical Sciences and Engineering Chemical Engineering Chemical Engineering (General)
Authors
,