Abstract
A new recycling process, according to the zero-waste concept, was investigated for an iron rich waste stream, more specifically a secondary lead smelting matte. The process consists of a selective citrate leaching of Pb, Cu, Ni and Zn in combination with a roasting step, leading to a simultaneous recovery of hematite as a secondary iron resource. The parameters, such as leaching time, leaching temperature, H2O2 concentration and roasting temperature, were experimentally optimized. The maximum Pb leaching efficiency was 93% and the leachability of Cu (33%) and Zn (11%) increased slightly in the presence of 0.5 M H2O2 in 1 M citrate at 25 °C and pH 5.5. Importantly, almost no Fe was leached (< 0.6%) from the iron rich matrix material at this condition allowing for a maximal recovery of hematite as a secondary resource after further treatment (i.e. roasting or sulfur removal). The leachability of Pb, Cu, Ni and Zn was strongly affected by the roasting temperature. Maximum leaching efficiency in 1 M citrate (25 °C, L/S ratio 10, pH 6.5) was 93% for Pb, 80% for Cu and 60% for Zn at a roasting temperature of 600 °C, while for Ni the maximum leaching efficiency of 53% was reached after roasting at 650 °C. Furthermore, when oxidative roasting was applied, the leaching residue consists dominantly of hematite (Fe2O3) with minor quantities of PbSO4, which can be used as pig iron ore (Fe > 60 wt%).
Related Topics
Physical Sciences and Engineering Chemical Engineering Chemical Engineering (General)
Authors
, , , , , ,