Article ID Journal Published Year Pages File Type
49872 Catalysis Communications 2015 5 Pages PDF
Abstract

•Preparation of MnxW0.05Ti0.95 − xO2 − δ by solution combustion method•High NH3-SCR activity in a wide temperature range•Formation of MnWOx phase is a key factor

A series of TiO2 supported MnWOx catalysts MnxW0.05Ti0.95 − xO2 − δ (x = 0.05, 0.1, 0.15) were synthesized by solution combustion method. The Mn0.10W0.05Ti0.85O2 − δ catalyst showed highest activity in NH3-SCR reaction within a broad temperature range of 200 °C–400 °C. XRD and TEM results indicate that the active Mn and W species are highly dispersed over TiO2 support in the form of nanoparticles (4–7 nm). The TEM and H2-TPR results also suggest that a MnWOx phase has been formed on the TiO2, which is beneficial for the activity of the MnxW0.05Ti0.95 − xO2 − δ catalysts in the high temperature range of 280 °C–400 °C.

Graphical abstractFigure optionsDownload full-size imageDownload as PowerPoint slide

Related Topics
Physical Sciences and Engineering Chemical Engineering Catalysis
Authors
, , , , ,