Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
5143797 | Organic Electronics | 2017 | 4 Pages |
Abstract
PEDOT:PSS/SWCNT composites can be prepared by mixing aqueous dispersions of PEDOT:PSS and SWCNT at different weight ratios. By being soaked with DMSO for 2 min at room temperature, the PEDOT:PSS/SWCNT composite with an optimized SWCNT weight ratio of 74 wt% exhibits a promising power factor of 300 μW mâ1 Kâ2, which is the highest among PEDOT:PSS and CNT composites.299
Related Topics
Physical Sciences and Engineering
Chemistry
Chemistry (General)
Authors
Lu Zhang, Yutaka Harima, Ichiro Imae,