At high strains, above e = 1, an advanced crystallographic slip and high stretch of amorphous material due to interlamellar shear bring further heavy fragmentation of lamellar crystals, earlier fragmented partially by deformation bands. This fragmentation is followed by fast rotation of small unconstrained crystallites with chain axis towards the direction of flow, FD. This process leads to development of the final texture of the highly deformed β-iPP with molecular axis of both crystalline and smectic phases oriented along FD.