Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
5191265 | Polymer | 2005 | 6 Pages |
Abstract
4,4â²-Bis(3,4-dicarboxyphenylthio)diphenyl sulfone dianhydride(4,4â²-PTPSDA) and 4,4â²-bis(2,3-dicarboxyphenylthio)diphenyl sulfone dianhydride(3,3â²-PTPSDA) were synthesized from chlorophthalic anhydrides and bis(4-mercaptophenyl)sulfone. Their structures were determined via IR spectra, 1H NMR and elemental analysis. A series of polyimides were prepared from isomeric PTPSDAs and aromatic diamines in 1-methyl-2-pyrrolidinone (NMP) via the conventional two-step method. Polyimides based on 4,4â²-PTPSDA and 3,3â²-PTPSDA have good solubility in polar aprotic solvents and phenols. The 5% weight-loss temperatures of isomeric polyimides were near 500 °C in N2. DMTA and DSC analyses indicated that the glass-transition temperatures of polyimides from 3,3â²-PTPSDA are higher than those of polyimides from 4,4â²-PTPSDA. The wide-angle X-ray diffraction showed that all polyimides are amorphous. The polyimides from 3,3â²-PTPSDA showed higher permeability but lower permselectivity compared with those from 4,4â²-PTPSDA.
Related Topics
Physical Sciences and Engineering
Chemistry
Organic Chemistry
Authors
Jingling Yan, Zhen Wang, Lianxun Gao, Mengxian Ding,