Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
5202920 | Polymer Degradation and Stability | 2011 | 7 Pages |
Abstract
Fracture toughness tests showed an increase of the KIC value with the increase of the toughening agent concentration, revealing both a dramatic decrease of the same parameter after 1 week ageing for all the materials and the tendency to reach an almost constant value after 1 month ageing for all the formulations, with a slight increase with respect to 1 week ageing. These results have been interpreted on the basis of the SEM analysis, showing the presence of a well defined micrometric PES particles distribution in the epoxy/anhydride matrix, and discussed in the light of different water absorption mechanisms at short and long ageing times.
Related Topics
Physical Sciences and Engineering
Chemistry
Organic Chemistry
Authors
S. Alessi, D. Conduruta, G. Pitarresi, C. Dispenza, G. Spadaro,