Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
5204609 | Polymer Degradation and Stability | 2007 | 9 Pages |
Abstract
As far as nanocomposite characteristics are concerned, the latter have been found to depend on both the preparation method and clay type. In the case of in situ polymerization, also thermally-treated layered silicates, coded (T), have been used, in order to put more clearly in evidence the role of compatibilizer decomposition on nanocomposite formation and properties. Indeed, nanocomposite samples containing Closite 30B®(T) have been found to be completely exfoliated, while the same thermal treatment seems to make worse the properties of those based on Nanofil 784®(T). Furthermore, with respect to nanocomposites based on pristine clays, samples containing thermally-treated silicates turned out to be different in terms of both molecular mass and crystal structure of the polymer matrix. Namely, PA6 γ-form seems to be promoted for all nanocomposites prepared in such a way, probably because of water removal at high temperature, which makes -OH groups of the layered silicate more free to interact with polyamide chains, thus causing a restriction of their mobility.
Keywords
Related Topics
Physical Sciences and Engineering
Chemistry
Organic Chemistry
Authors
Orietta Monticelli, Zenfira Musina, Alberto Frache, Federica Bellucci, Giovanni Camino, Saverio Russo,