The thermal stability of starch cross-linked with tetraethylene glycol diacrylate was studied under nitrogen atmosphere by thermogravimetry (TG) and infrared spectroscopy (FTIR). The cross-linking reaction was confirmed by the increase in intensity of the absorption band at ca. 3330 cmâ1 indicating the reinforcement of hydrogen bonds and the appearance of a new band at 1726 cmâ1 associated with the carbonyl group of the cross-linking agent. After cross-linking the solubility of starch in water decreased to the range 9%-16%. The thermogravimetric curves of pure and cross-linked starches showed an initial stage of degradation (up to ca. 150 °C) associated with the loss of water. The main stage of degradation occurred in the range 250-400 °C corresponding to ca. 60%-70% mass loss. The activation energy (E) for the degradation process increased from 145 kJ molâ1 (pure starch) to 195 kJ molâ1 and 198 kJ molâ1 for starch treated for 60 min by UV (30 °C) and at 90 °C, suggesting high stability after cross-linking. A higher value (240 kJ molâ1) was obtained for starch treated by UV for 120 min. The main volatile products determined by FTIR which correspond to hydrocarbons and carbonyl groups are apparently associated with the scission of weak bonds in the chain (probably branched groups) and the scission of stronger bonds (glycosidic linkages), respectively.
Related Topics
Physical Sciences and Engineering
Chemistry
Organic Chemistry
Authors
P.T. Marques, A.M.F. Lima, G. Bianco, J.B. Laurindo, R. Borsali, J.-F. Le Meins, V. Soldi,