| Article ID | Journal | Published Year | Pages | File Type |
|---|---|---|---|---|
| 5206814 | Polymer Testing | 2012 | 7 Pages |
Abstract
Results show that if FU and FÉ >1, the PCM sample would have sufficient formability under the drawing condition. However, the tensile strength of film, if below the compressive stress of the deep drawing punch or die, also determines the success of forming in the drawing test.