| Article ID | Journal | Published Year | Pages | File Type |
|---|---|---|---|---|
| 5348162 | Applied Surface Science | 2016 | 8 Pages |
Abstract
The surface roughness (Ra) dropped from 38.23Â nm to 16.13Â nm after plasma treatment. No cracks appeared around crater c, which indicated preferable vertical adhesion was achieved through the transition layer.
Related Topics
Physical Sciences and Engineering
Chemistry
Physical and Theoretical Chemistry
Authors
F.F. He, W.Q. Bai, L.L. Li, X.L. Wang, Y.J. Xie, G. Jin, J.P. Tu,