⺠TIG surface alloying of AZ91D with Al + Ni caused formation of hard intermetallics. ⺠The hardness of the alloyed layer reached to 162 HV which was twice of that of AZ91D. ⺠Wear rate of alloyed layer was reduced to half of the wear rate of untreated AZ91D.