Abstract
⺠WS2 is utilized to produce high temperature self-lubricant wear-resistant composite coating by laser cladding. ⺠Noticeably, the coating added withWS2 has a higher microhardness because of the formation of the hard phase (Cr,W)C. ⺠The average friction coefficients both decrease with the rising of temperature, but the wear rates both increase. ⺠The coating added with WS2 has a lower friction coefficient whatever at ambient, 300 °C, 600 °C, and a lower wear rate only at 300 °C.