Article ID Journal Published Year Pages File Type
5370439 Applied Surface Science 2006 6 Pages PDF
Abstract
Oxidation protective SiC-Al2O3-mullite multi-coatings for carbon/carbon (C/C) composites were prepared with a two-step pack cementation process. The influence of preparation temperature and SiO2/Al2O3 ratio of the pack powder on the phase, microstructure and oxidation resistance of the multi-coatings were investigated. It showed that the multi-coatings that contained mullite could be produced at 1700-1800 °C. A denser coating surface was acquired with the decrease of SiO2/Al2O3 ratio in the pack chemistries while a little damnification to the interface of the coating and C/C substrate. The as-prepared coating could effectively protect C/C composites from oxidation at 1600 °C for 81 h.