Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
5387873 | Chemical Physics Letters | 2008 | 4 Pages |
Abstract
1Â ÃÂ 1Â mm2 SEM topography image of a P-doped polycrystalline diamond film grown using 800Â ppm [PH3]/[CH4]. The used doping conditions differ significantly from the ones used for P-doping of single crystal CVD diamond films.
Related Topics
Physical Sciences and Engineering
Chemistry
Physical and Theoretical Chemistry
Authors
A. Lazea, V. Mortet, J. D'Haen, P. Geithner, J. Ristein, M. D'Olieslaeger, K. Haenen,