| Article ID | Journal | Published Year | Pages | File Type |
|---|---|---|---|---|
| 5403853 | Journal of Luminescence | 2007 | 4 Pages |
Abstract
Starting from metal nitrate aqueous solutions and H3BO3, Y0.9âxGdxEu0.1Al3(BO3)4 (0⩽x⩽0.9) phosphors were synthesized by spray pyrolysis followed by annealing at high temperature. The obtained phosphor particles have spherical morphology with size in the range 0.5-2 μm. Independent of the x values in Y0.9âxGdxEu0.1Al3(BO3)4 (0⩽x⩽0.9) phosphors, the Eu3+ ion shows its characteristic 5D0, 1-7FJ (J=0, 1, 2, 3, 4) transitions with 5D0-7F2 red emission (612 nm) as the most prominent group. The photoluminescence intensity of phosphors increases with the increase of x value in Y0.9âxGdxEu0.1Al3(BO3)4 (0⩽x⩽0.9) due to an energy migration process like Gd3+-(Gd3+)n-Eu3+ that occurred in the host materials.
Keywords
Related Topics
Physical Sciences and Engineering
Chemistry
Physical and Theoretical Chemistry
Authors
L.S. Wang, X.M. Liu, Z.W. Quan, D.Y. Kong, J. Yang, J. Lin,