Brazing of Ti2AlC ceramics has been successfully performed using a pure Al filler metal, in the temperature range 1023Â K-1173Â K and with holding time ranging from 0 to 30Â min. The microstructure of the Ti2AlC joints was studied, and the mechanical properties of the joints were evaluated by shear strength test. It is observed that the Al filler has weak effect on the stability of Ti2AlC substrate, and only a small amount of decomposition products including the TiCx and TiAl3 compounds can be observed in the joints. In addition, the formation of an inter-diffusion layer in the Ti2AlC substrate is considered as the major brazing mechanism. The maximum shear strength of the Ti2AlC joints using the pure Al filler metal is 95Â MPa, with an electrical conductivity of 2.21Ã106Â SÂ mâ1, after holding the sample at 1123Â K for 10Â min.
Related Topics
Physical Sciences and Engineering
Materials Science
Ceramics and Composites
Authors
Chengjie Lu, Liangbo Sun, Jie Zhang, Qin Qi, Gilles Hug,