A new facility for the measurement of AC loss in superconductors at high dB/dt has been developed. The test device has a spinning rotor consisting of permanent magnets arranged in a Halbach array; the sample, positioned outside of this, is exposed to a time varying AC field with a peak radial field of 0.566 T. At a rotor speed of 3600 RPM the frequency of the AC field is 240 Hz, the radial dB/dt is 543 T/s and the tangential dB/dt is 249 T/s. Loss is measured using nitrogen boiloff from a double wall calorimeter feeding a gas flow meter. The system is calibrated using power from a known resistor. YBCO tape losses were measured in the new device and compared to the results from a solenoidal magnet AC loss system measurement of the same samples (in this latter case measurements were limited to a field of amplitude 0.1 T and a dB/dt of 100 T/s). Solenoidal magnet system AC loss measurements taken on a YBCO sample agreed with the Brandt loss expression associated with a 0-0.1 T Ic of 128 A. Subsequently, losses for two more YBCO tapes nominally identical to the first were individually measured in this spinning magnet calorimeter (SMC) machine with a Bmax of 0.566 T and dB/dt of up to 272 T/s. The losses, compared to a simplified version of the Brandt expression, were consistent with the average Ic expected for the tape in the 0-0.5 T range at 77 K. The eddy current contribution was consistent with a 77 K residual resistance ratio, RR, of 4.0. The SMC results for these samples agreed to within 5%. Good agreement was also obtained between the results of the SMC AC loss measurement and the solenoidal magnet AC loss measurement on the same samples.
Related Topics
Physical Sciences and Engineering Materials Science Electronic, Optical and Magnetic Materials
Authors
, , , , , , ,