Article ID Journal Published Year Pages File Type
5454791 Materials Characterization 2017 19 Pages PDF
Abstract
Cast-rolling AZ31 Mg alloy sheets were manufactured at four rolling speed ratios of 0.8, 1.0, 1.2 and 1.3. The results show that the basal texture can be weakened by differential speed rolling (DSR). The AZ31 alloy sheet manufactured at a speed ratio of 1.2 exhibits a fine microstructure with an average grain size of 10.3 μm. The yield strength, ultimate tensile strength and elongation-to-failure at this speed ratio are 145 MPa, 240 MPa and 28.5% at room temperature, respectively. These parameters mainly benefit from the fine grains and weakened basal texture. The AZ31 alloy sheets processed by the DSR exhibit a remarkable improvement in elongation-to-failure compared with the AZ31 alloy sheets processed by equal speed rolling (ESR) primarily due to the weakened basal texture at room temperature. However, the difference in elongation-to-failure of the AZ31 alloy sheets processed by the ESR and DSR decreases at elevated temperatures, which can be attributed to the weakening of the influence of basal texture, with probable activation of non-basal slips and grain boundary sliding (GBS). The results obtained here will shed light on some DSR methods, which is critical to the development of Mg alloys with high mechanical properties.
Related Topics
Physical Sciences and Engineering Materials Science Materials Science (General)
Authors
, , , , , , ,